东北大学学报:自然科学版 ›› 2020, Vol. 41 ›› Issue (8): 1148-1152.DOI: 10.12068/j.issn.1005-3026.2020.08.014

• 材料与冶金 • 上一篇    下一篇

车轮轮辐钢S500LF的疲劳性能

高彩茹1, 朱长友1, 张大伟1,2, 杜林秀1   

  1. (1. 东北大学 轧制技术及连轧自动化国家重点实验室, 辽宁 沈阳110819; 2. 首钢技术研究院 薄板研究所, 北京100043)
  • 收稿日期:2019-07-24 修回日期:2019-07-24 出版日期:2020-08-15 发布日期:2020-08-28
  • 通讯作者: 高彩茹
  • 作者简介:高彩茹(1965-),女,内蒙古赤峰人,东北大学副教授,博士.
  • 基金资助:
    国家高技术研究发展计划项目(2015AA03A501).

Fatigue Property of Spoke Steel S500LF

GAO Cai-ru1, ZHU Chang-you1, ZHANG Da-wei1,2, DU Lin-xiu1   

  1. 1. State Key Laboratory of Rolling Technology and Automation, Northeastern University, Shenyang 110819, China; 2. Sheet Research Institute, Shougang Research Institute of Technology, Beijing 100043, China.
  • Received:2019-07-24 Revised:2019-07-24 Online:2020-08-15 Published:2020-08-28
  • Contact: GAO Cai-ru
  • About author:-
  • Supported by:
    -

摘要: 采用PX-100高频疲劳试验机,采用升降法在振动频率为100~120Hz、拉-压对称应力的条件下测定车轮轮辐钢S500LF的疲劳极限,并用数理统计方法分析确认疲劳极限为291MPa.此值作为母体50%存活率下的疲劳极限估计量时,以95%的置信度,相对误差不超过±5%.在测定的疲劳极限基础上,采用多试样法测得不同应力水平下的疲劳寿命,据此绘制出应力-寿命关系曲线,通过回归得到应力-寿命曲线方程.对试样断口进行了理论分析,结果表明试验钢韧性良好.

关键词: 轮辐钢, 疲劳极限, S-N曲线, 疲劳断口

Abstract: An experiment was carried out on the high frequency fatigue testing machine PX-100 and with the method of progressively increasing/decreasing stress to determine the fatigue limit of wheel spoke steel S500LF on the condition that the vibration frequency was 100~120Hz and the tensile-compressive stress was symmetrical. The fatigue limit was 291MPa by the mathematical statistical analysis. When this value was used as an estimator of the maternal 50% survival rate, the relative error was no more than ±5% with a confidence level of 95%. The fatigue life at different stress levels was measured by the multi-sample method according to the measured fatigue limit. Based on this, the S-N relation curve was drawn and the S-N curve equation was regressed. Besides, the fracture of the samples was analyzed theoretically, and the result shows the good toughness of the test steel.

Key words: spoke steel, fatigue limit, S-N curve, fatigue fracture