东北大学学报(自然科学版) ›› 2023, Vol. 44 ›› Issue (2): 206-214.DOI: 10.12068/j.issn.1005-3026.2023.02.008

• 材料与冶金 • 上一篇    下一篇

铁精粉制备α-Fe2O3纳米粒子及其机理

李婷1,2, 裴文利1,2, 陈婉晴3, 佟冰3   

  1. (1. 东北大学 材料科学与工程学院, 辽宁 沈阳110819; 2. 东北大学 材料各向异性与织构教育部重点实验室, 辽宁 沈阳110819; 3. 抚顺罕王傲牛矿业股份有限公司, 辽宁 抚顺113125)
  • 修回日期:2021-12-07 接受日期:2021-12-07 发布日期:2023-02-27
  • 通讯作者: 李婷
  • 作者简介:李婷(1996-),女,福建南平人,东北大学硕士研究生; 裴文利(1970-),男,辽宁沈阳人,东北大学教授,博士生导师.
  • 基金资助:
    国家自然科学基金资助项目(52071070, 51871045); 中央高校基本科研业务费专项资金资助项目(N2017003, N2102004).

Preparation and Mechanism of α-Fe2O3 Nanoparticles by Using Iron Concentrate Powder

LI Ting1,2, PEI Wen-li1,2, CHEN Wan-qing3, TONG Bing3   

  1. 1. School of Material Science & Engineering, Northeastern University, Shenyang 110819, China; 2. Key Laboratory for Anisotropy and Texture of Materials Ministry of Education, Northeastern University, Shenyang 110819, China; 3. Fushun Hanking Aoniu Mining Co., Ltd., Fushun 113125, China.
  • Revised:2021-12-07 Accepted:2021-12-07 Published:2023-02-27
  • Contact: PEI Wen-li
  • About author:-
  • Supported by:
    -

摘要: 采用商业磁铁矿铁精粉(Fe3O4),设计了提纯和制备工艺,成功制备出质量分数为99.5%以上、分散性良好的α-Fe2O3纳米粒子,对其提纯、制备工艺及机理进行了深入研究. 结果表明:w○NaOH对除硅效果影响显著, 当w○NaOH为39 %时,可使原料矿粉中w○SiO▲2由1.11 %降至0.032%, 得到较纯铁精粉;随烧结温度的升高, α-Fe2O3颗粒的结晶度、形貌特征及磁性能随之发生变化;当烧结温度为670℃时, α-Fe2O3颗粒综合性能最佳,颗粒结晶度较高、分散性较好,具有亚铁磁性;通过对氢氧化铁沉淀物加热搅拌时间的控制,可有效调控α-Fe2O3的晶粒尺寸;当搅拌时间为60min时, 获得分散性好、平均粒径仅为35.3nm的α-Fe2O3纳米粒子.

关键词: α-Fe2O3;铁精粉;纳米颗粒;晶粒尺寸;分散性

Abstract: Using commercial magnetite iron powder(Fe3O4), a purification and preparation process was designed, and α-Fe2O3 nanoparticles with a mass fraction of more than 99.5% and good dispersibility were successfully prepared. The purification, preparation process and mechanism were studied in detail. The results show that: wNaOH has a significant impact on the effect of silicon removal, when wNaOH is 39 %, the wSiO▲2 in the raw ore powder can be reduced from 1.11 % to 0.032 % to get more pure iron fine powder. With the increase of the sintering temperature, the crystallization, appearance characteristics and magnetic properties of α-Fe2O3 particles have changed. When the sintering temperature is 670℃, the comprehensive performance of α-Fe2O3 particles is the best, including higher particle crystallinity, good dispersibility and ferrimagnetic properties. By controlling the heating and stirring time of the hydroxide sediment, the grain size of the α-Fe2O3 can be effectively regulated. When the stirring time is 60min, the α-Fe2O3 with a high-quality dispersability and a average particle size of only 35.3nm is obtained.

Key words: α-Fe2O3; iron concentrate powder; nanoparticles; grain size; dispersion