GONG Wei, WANG Cheng, WANG Haidong, JIANG Zhouhua. Inclusions Modification in Die Steel with Magnesium Vapor[J]. Journal of Northeastern University Natural Science, 2014, 35(5): 704-707.
[1] Chen Z Z,Ma D S.Analysis of development strategy for national die steel industry[J].Iron and Steel,2005,70(4):22/27. [2] tatharas D,Papageorgiou D,Sideris J,et al.Preliminary examination of the fracture surfaces of a cold working die[J].International Journal of Material Forming,2008,1(5):431/434. [3] Okolovich G A.Tool steels for cold working dies[J].Metal Science and Heat Treatment,2006,48(3):5/6. [4] Statharas D,Sideris J,Medrea C,et al.Microscopic examination of the fracture surfaces of a cold working die due to premature failure[J].Engineering Failure Analysis,2011,18(2):759/765. [5] Fegredo D M,Shehata M T,Palmer A,et al.The effect of sulphide and oxide inclusions on the wear rates of a standard CMn and a CrMo alloy rail steel[J].Wear,1998,126(3):285/306. [6] Bolton P J,Clayton P.Rollingsliding wear damage in rail and tire steels[J].Wear,1984,93(2):145/165. [7] Kubota K,Ohba T,Morito S.Frictional properties of new developed cold work tool steel for high tensile strength steel forming die[J].Wear,2011,271(3):2884/2889. [8] 吴年强,李志章.夹杂物对Cr13铸钢耐磨性的影响[J].浙江大学学报:自然科学版,1997,31(1):17/22.(Wu Nianqiang,Li Zhizhang.Effects of inclusion on wear resistance of the Cr13 cast steels[J].Journal of Zhejiang University:Natural Science,1997,31(1):17/22.) [9] Yang J,Yamasaki T,Kuwabara M.Behavior of inclusions in deoxidation process of molten steel with in situ produced magnesium vapor[J].ISIJ International,2007,47(5):699/708. [10] Takata R,Yang J,Kuwabara M.Charcteristics of inclusions generated during AlMg complex deoxidation of molten steel[J].ISIJ International,2007,47(10):1379/1386.