1. School of Materials & Metallurgy, Northeastern University, Shenyang 110819, China; 2. Zhenzhou Research Institute of China Aluminum Corporation, Zhenzhou 450041, China.
ZHANG Juhua, ZHANG Wei, ZHANG Li, GU Songqing. Effect of Acid Leaching on the Vanadium Leaching Rate in Process of Vanadium Extraction Using Calcium Roasting[J]. Journal of Northeastern University Natural Science, 2014, 35(11): 1574-1577.
[1]廖世明,柏谈论.国外钒冶金[M].北京:冶金工业出版社,1985:4-19.(Liao Shiming,Bai Tanlun.Foreign vanadium metallurgy[M].Beijing:Metallurgical Industry Press,1985:4-19.) [2]Moskalyk R R,Alfantazi A M.Processing of vanadium:a review[J].Minerals Engineering,2003,16(9):793-805. [3]Polyak D E.U S 2009 minerals yearbookvanadium[M].Reston:Geological Survey,2011:1-10. [4]Zhang Y M,Hu Y J,Bao S X.Vanadium emission during roasting of vanadiumbearing stone coal in chloride[J].Minerals Engineering,2012,30:95-98. [5]Du J,Wang N,Tao C Y,et al.Microwaveaided roasting for extraction of vanadium from stone coal[J].Chemical Industry and Engineering Progress,2010,29(sup1):494-497. [6]Li X S,Xie B,Wang G E.Oxidation process of lowgrade vanadium slag in presence of Na2CO3[J].Transitions Nonferrous Metals Society of China,2011,21(8):1860-1867. [7]Chen T J,Zhang Y M,Song S X.Improved extraction of vanadium from a Chinese vanadiumbearing stone coal using a modified roastleaching process[J].Asiapacific Journal of Chemical Engineering,2010,5:778-784. [8]Wang F,Zhang Y M,Liu T,et al.Comparison of direct acid leaching process and blank roasting acid leaching process in extracting vanadium from stone coal[J].International Journal of Mineral Processing,2014,128:40-47. [9]Liu B,Du H,Wang S N.A novel method to extract vanadium and chromium from vanadium slag using molten NaOHNaNO3 binary system[J].AIChE Journal,2013,59(2):541-552. [10]Rakib M,Durand G.Study of complex formation of vanadium(V)with sulphate ions using a solvent extraction method[J].Hydrometallurgy,1996,43(1/2/3):355-366. [11]张菊花.改性高钛渣中金红石相的分离研究[D].沈阳:东北大学,2009.(Zhang Juhua.Separation of rutile phase in the modified high titanium slag[D].Shenyang:Northeastern University,2009.)(上接第1573页)3结论1) 澄清室的分散相厚度随着时间的增大而减小,并且澄清室有搅拌比无搅拌能有效缩短分散相厚度到达稳态的时间.2) 澄清室出口的相夹带随时间的增大而减小,并且澄清室有搅拌与澄清室无搅拌时油相出口的水相夹带区别不大,水相出口的油相夹带明显较小.3) 数值模拟得到的速度场与PIV实测得到的速度场保持一致.澄清室有搅拌时比无搅拌时更有效地抑制回流,能加速油、水两相分离.