Journal of Northeastern University ›› 2013, Vol. 34 ›› Issue (3): 399-402.DOI: -

• Materials & Metallurgy • Previous Articles     Next Articles

Pretreatment of Copper Anode Slime with High Nickel Content for Concentrating Gold and Silver

YANG Hongying, CHEN Guobao, PENG Yufeng, LI Xuejiao   

  1. School of Materials & Metallurgy, Northeastern University, Shenyang 110819, China.
  • Received:2012-09-24 Revised:2012-09-24 Online:2013-03-15 Published:2013-01-26
  • Contact: YANG Hongying
  • About author:-
  • Supported by:
    -

Abstract: Taking the typical refractory high nickel copper anode slime as the raw material, the effects of temperature, time and liquidsolid ratio etc. factors on the removal of the metals selenium, copper and nickel were studied. The results showed that, after roastingleaching twice, 995% of selenium, 997% of copper, 9335% of nickel were removed. 9876% silver was in the leaching solution, and the amount of gold reached 1820g·t-1 from 193g·t-1. The best conditions of the first roastingleaching process were as follows, the roasting temperature of 650℃, the roasting time of 1h, m(H2SO4)/m(anode slime) of 12, the leaching temperature of 55℃, the leaching time of 1h, and the liquidsolid ratio of 6. The best conditions of the second roastingleaching process were as follows, the roasting temperature of 500℃, m(H2SO4)/m(anode slime) of 12, the roasting time of 3h, the leaching temperature of 55℃, the leaching time of 1h and the liquidsolid ratio of 6. The weight of the anode slime decreased to 1126% that of the original after the pretreatment, which greatly enhanced the handling capacity of the equipment during the subsequent recovery process.

Key words: copper anode slime with high nickel content, pretreatment, gold, sulfurizing roasting process, acid leaching