Regeneration-Modification of Deactivated V2O5-based Catalyst Used for Low Load Condition Denitration
SHANG Da1,2, LI Bao-kuan1
1.School of Metallurgy, Northeastern University, Shenyang 110819, China; 2.Science and Technology Development Co., Ltd., China Energy Engineering Group, Tianjin 300012, China.
SHANG Da, LI Bao-kuan. Regeneration-Modification of Deactivated V2O5-based Catalyst Used for Low Load Condition Denitration[J]. Journal of Northeastern University Natural Science, 2019, 40(6): 908-912.
[1]Zhang L,Zhang D S,Zhang J P,et al.Design of meso-TiO2@MnO○x-CeO○x/CNTs with a core-shell structure as DeNO○x catalysts:promotion of activity,stability and SO2 tolerance [J].Nanoscale,2013,5(20):9821-9829. [2]Zhang M H,Huang B J,Jiang H X,et al.Research progress in the SO2 resistance of the catalysts for selective catalytic reduction of NO○x [J].Chinese Journal of Chemical Engineering,2017,25(12):1695-1705. [3]Zheng K Z,Yang G H,Shen W J,et al.Preparation and denitration performance of V-W/TiO2-SiO2 nanotube catalysts [J].Water Air and Soil Pollution,2018,229(4):1-11. [4]Khodayari R,Odenbrand C U I.Regeneration of commercial TiO2-V2O5-WO3 SCR catalysts used in bio fuel plants [J].Applied Catalysis B—Environmental,2001,30(1/2):87-99. [5]Peng Y,Li J H,Si W Z,et al.Insight into deactivation of commercial SCR catalyst by arsenic:an experiment and DFT study [J].Environmental Science & Technology, 2014,48(23):13895-13900. [6]Li X,Li X S,Li J H,et al.High calcium resistance of CeO2-WO3 SCR catalysts:structure investigation and deactivation analysis [J].Chemical Engineering Journal,2017,317:70-79. [7]Xu T F,Wu X D,Liu X S,et al.Effect of barium sulfate modification on the SO2 tolerance of V2O5/TiO2 catalyst for NH3-SCR reaction [J].Journal of Environmental Sciences,2017,57:110-117. [8]Yu Y K,He C,Chen J S,et al.Regeneration of deactivated commercial SCR catalyst by alkali washing [J].Catalysis Communications,2013,39:78-81. [9]Panahi P N,Salari D,Niaei A,et al.Study of M-ZSM-5 nanocatalysts(M:Cu,Mn,Fe,Co...)for selective catalytic reduction of NO with NH3:process optimization by Taguchi method [J].Chinese Journal of Chemical Engineering,2015,23(10):1647-1654. [10]Yao X J,Kong T T,Chen L,et al.Enhanced low-temperature NH3-SCR performance of MnO○x/CeO2 catalysts by optimal solvent effect[J].Applied Surface Science,2017,420:407-415. [11]贾勇,周军,柏家串,等.砷、钾复合中毒选择性催化还原脱硝催化剂的再生[J].硅酸盐学报,2016,44(7):1025-1032.(Jia Yong,Zhou Jun,Bai Jia-chuan,et al.Hybrid regeneration of selective catalytic reduction denitration catalyst poisoned by arsenic and potassium[J].Journal of the Chinese Ceramic Society,2016,44(7):1025-1032.) [12]王丽霞,仲兆平,朱林,等.铁铈复合选择性催化还原脱硝催化剂的碱金属(钾)中毒机理[J].化工进展,2017,36(11):4064-4071.(Wang Li-xia,Zhong Zhao-ping,Zhu Lin,et al.Alkali metal(potassium)poisoning mechanism of CeFeO○x catalysts for selective catalytic reduction of NO○x [J].Chemical Industry and Engineering Progress,2017,36(11):4064-4071.) [13]Kong M,Liu Q C,Wang X Q,et al.Performance impact and poisoning mechanism of arsenic over commercial V2O5-WO3/TiO2 SCR catalyst[J].Catalysis Communications, 2015,72:121-126.